Naziha, LADJAL
(Université de m'sila, 2013-10-13)
Activated carbon were prepared by thermochemical activation at 450 °C of the shell of
apricot stone for varions ratios of impregnation of phosphoric acid : 30, 60, 90, 120,150 and
180 % by mass. These coals were ...